Thermal Shock Heat Test

Conventional sealants start to emulsify at rather low temperatures. Once the panel was treated with Ziridium Exterior Bond it was placed in a chamber and shocked multiple times at temperatures ranging from -10 to over 500 degrees.
Test Panels
SAMPLE WITH NO COATING - AFTER TESTING

Before

SAMPLE TREATED WITH ZIRIDIUM - AFTER TESTING

After

Ziridium showed zero deterioration.

Result
Passed