ACCELERATED UV EXPOSURE LEATHER BOND TEST 

The leather samples were treated with Ziridium Leather Bond and placed in an accelerated UV exposure chamber in accordance with ASTM G154-06.

Test Panels

SAMPLE WITH NO COATING - AFTER TESTING

SAMPLE TREATED WITH ZIRIDIUM - AFTER TESTING

Ziridium showed zero deterioration.

Result

Passed

There was zero surface degradation zero color change and zero chalking on any of the test of the treated samples.